Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
ASTM D2240
Tensile Strength, Ultimate 8.27 MPa
1200 psi
ASTM D412
Tensile Strength, Yield 3.24 MPa
470 psi
at 100%; ASTM D412
Elongation at Break 670 %
670 %
ASTM D412
Tear Strength 40.3 kN/m
230 pli
die B; ASTM D624