GEHR Plastics ECOGEHR® PA 11 Nylon 11 Conditioned  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics ECOGEHR® PA 11 Nylon 11 Conditioned  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 11 is made 100% from the components of castor oil, and is thus wholly bio-based. ECOGEHR® Nylon 11 possesses similar properties to Nylon 12, and an excellent status with respect to applications that require thermal, physical, chemical and mechanical material properties. Good cold impact strength (down to -40 °F), good chemical resistance and low water absorption (only 1/6 in comparison with Nylon 6) are characteristics of the material.Information provided by GEHR Plastics, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Water Absorption 0.90 %
0.90 %
ASTM D570
Mechanical Properties Metric English Comments
Elongation at Break >= 200 %
>= 200 %
ASTM D1708
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
HDT/B; ASTM D648
Vicat Softening Point 180 °C
356 °F
VST/A/50; ASTM D1525
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
ELS Upgrade Yes
Industrially Biodegradable No
Renewable Content (%) 100