Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Comparative Tracking Index = 600 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
ASTM D2303
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Comparative Tracking Index >= 600 V
>= 600 V
UL 746
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Comparative Tracking Index 600 V
600 V
UL746A
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade  (discontinue
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit..
Comparative Tracking Index 600 V
600 V
IEC 60112
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA)  (Unverified Data**)
Ixef 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss. - B..
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:9
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Comparative Tracking Index 600 V
600 V
IEC 60112
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP
BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage..
Comparative Tracking Index 600 V
600 V
A solution
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Comparative Tracking Index 600 V
600 V
IEC 60112
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin.
Comparative Tracking Index 600 V
600 V
IEC 60112
Styrolution Novodur® E309 ABS
Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution
Comparative Tracking Index 600 V
600 V
IEC 60112
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific)
Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r..
Comparative Tracking Index 600 V

@Thickness 3.00 mm
600 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Comparative Tracking Index 600 V
600 V
Stufe; IEC 112
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30
Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X..
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)
43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Comparative Tracking Index 600 V

@Thickness 3.00 mm,
Temperature 23.0 °C
600 V

@Thickness 0.118 in,
Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Comparative Tracking Index 600 V
600 V
IEC 60112
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar.
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
EMS-Grivory Grivory® LKN-3H PA12-GB30
Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
Comparative Tracking Index 600 V
600 V
Arkema Group Orgalloy® LE 60XV Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).Suited to the extrusion of tubes (hydraulic, pneumatic, painting.....
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Comparative Tracking Index 600 V
600 V
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.
Comparative Tracking Index 600 V
600 V
Test Solution A; IEC 60112
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Comparative Tracking Index >= 600 V

@Temperature 23.0 °C
>= 600 V

@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
600 V
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material
QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi..
Comparative Tracking Index 600 V
600 V
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Comparative Tracking Index 600 V
600 V
BASF Novolen® 1148 RC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
Comparative Tracking Index 600 V
600 V
IEC 60112
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an..
Comparative Tracking Index 600 V

@Temperature 23.0 °C
600 V

@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad..
Comparative Tracking Index 600 V
600 V
Solution A, Rating; IEC 60112
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Copyright © lookpolymers.com All Rights Reserved