Material Notes:
Nylon 6.10 is 60 % sebacic acid, which is obtained from castor oil. This material combines a low density (for polyamide) with good cold impact strength, and its low water absorption makes it very dimensionally stable. This is in addition to a very high (for bio-based polymers) continuous usage temperature of 212°F and its chemical resistance to organic solvents, for which PA is well known. This material can thus be used not only in traditional Nylon 6 applications, but also where the use of Nylon 6 previously reached its limits.Information provided by GEHR Plastics, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.4 %
1.4 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Yield 20 %
20 %
Modulus of Elasticity 1.30 GPa
188 ksi
ASTM D638
Izod Impact, Notched (ISO) 88.2 kJ/m²
42.0 ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO) NB
NB
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
HDT/A; ASTM D648
Descriptive Properties Value Comments
Industrially Biodegradable No
Renewable Content (%) 63
Users viewing this material also viewed the following: