Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GRECO ISOPAK 569 ABS Resin

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer GRECO
Trade Name ISOPAK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOPAK 569 ABS Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Water Absorption 0.30 %

@Temperature 23.0 °C,
Time 86400 sec
0.30 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 0.50 - 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.50 - 1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength 44.1 MPa
6400 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D412
Flexural Yield Strength 68.6 MPa
9960 psi
ASTM D790
Flexural Modulus 2.26 GPa
327 ksi
ASTM D790
Izod Impact, Notched 3.33 J/cm
6.25 ft-lb/in
ASTM D256 A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL-746B
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 15 sec
15 sec
.062" and above; UL-746A
High Amp Arc Ignition, HAI 200 arcs
200 arcs
.062" and above; UL-746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/min
0.000 in/min
.062" and above; UL-746A
Users viewing this material also viewed the following: