Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 44.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 44.1 MPa
6400 psi
ASTM D412
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane
ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon.
Tensile Strength 44.1 MPa
6400 psi
ASTM D412
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon.
Tensile Strength 44.1 MPa
6400 psi
ASTM D412
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Tensile Strength 44.1 MPa
6400 psi
ASTM D412
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry Parts Information provided by API-Kolon.
Tensile Strength 44.1 MPa
6400 psi
ASTM D638
GRECO ISOPAK 569 ABS Resin
Extrusion GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Tensile Strength 44.1 MPa
6400 psi
50 mm/min; ISO 527-1,-2
Gromax BTE35-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength >= 44.1 MPa
>= 6400 psi
ASTM D 638
Karina E 786-10/332-IS-RG Compound PVC White
White rigid for spiral hoses (non-toxic)Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 44.1 MPa
6400 psi
50 mm/min; ISO 527-1,-2
Gromax ATE70-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 44.1 MPa
6400 psi
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
Tensile Strength 44.1 MPa
6400 psi
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 44.1 MPa
6400 psi
Taiwan Sheen Soon Sheenthane® D6320E Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 44.1 MPa
6400 psi
Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 44.1 MPa
6400 psi
Taiwan Sheen Soon Sheenthane® A9720E Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 44.1 MPa
6400 psi
ASTM D638
Samyang Trimma® SD6320 PMMA, Translucent
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Tensile Strength 44.1 MPa

@Temperature 23.0 °C
6400 psi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Tensile Strength 44.1 MPa
6400 psi
ASTM D638
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene
Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC.
Tensile Strength 44.1 - 57.9 MPa
6400 - 8400 psi
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound
BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o..
Copyright © lookpolymers.com All Rights Reserved