GRECO ISOTHANE 1065D Poly(adipate)ester TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 1065D Poly(adipate)ester TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
Tensile Strength, Yield 19.0 MPa

@Strain 50.0 %
2760 psi

@Strain 50.0 %
ASTM D412
21.0 MPa

@Strain 100 %
3050 psi

@Strain 100 %
ASTM D412
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ASTM D412
Elongation at Break 440 %
440 %
ASTM D412
Tear Strength 240 kN/m
1370 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 15
15
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395