Polymer Property : Tensile Strength, Yield = 3050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa

@Strain 50.0 %
3050 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 21.0 MPa

@Strain 50.0 %
3050 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1095AE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength, Yield 21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3090A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 21.0 MPa

@Strain 100 %
3050 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1065D Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 21.0 MPa

@Temperature 121 °C
3050 psi

@Temperature 250 °F
ASTM D638
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Tensile Strength, Yield 21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Yield 21.0 MPa

@Strain 100 %
3050 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..