GRECO ISOTHANE 1195A Poly(adipate)ester TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 1195A Poly(adipate)ester TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transparency. These products can be injection molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength 38.0 MPa
5510 psi
ASTM D412
Tensile Strength, Yield 7.60 MPa

@Strain 50.0 %
1100 psi

@Strain 50.0 %
ASTM D412
9.70 MPa

@Strain 100 %
1410 psi

@Strain 100 %
ASTM D412
17.0 MPa

@Strain 300 %
2470 psi

@Strain 300 %
ASTM D412
Elongation at Break 570 %
570 %
ASTM D412
Tear Strength 120 kN/m
685 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 30
30
ASTM D1044(Taber) H-22