Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 2470 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa

@Temperature 121 °C
2470 psi

@Temperature 250 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 17.0 MPa

@Strain 300 %
2470 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1195A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 3055D Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 17.0 MPa

@Strain 300 %
2470 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3090AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 17.0 MPa

@Strain 300 %
2470 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 5090A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1170D Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 17.0 MPa

@Strain 50.0 %
2470 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 17.0 MPa

@Strain 50.0 %
2470 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Copyright © lookpolymers.com All Rights Reserved