GRECO ISOTHANE 1685AE Polyether TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 1685AE Polyether TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Water Vapor Transmission 9000 g/m²/day
580 g/100 in²/day
ASTM E-96BW
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 30.5 MPa
4420 psi
ASTM D412
Tensile Strength, Yield 9.40 MPa

@Strain 300 %
1360 psi

@Strain 300 %
ASTM D412
Elongation at Break 735 %
735 %
ASTM D412
Tear Strength 8.80 kN/m
50.2 pli
ASTM D624