Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D412 |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D638 |
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D638 |
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Tensile Strength, Yield | 9.40 MPa @Strain 300 % |
1360 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1685AE Polyether TPU Resin ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf.. |
|||
Tensile Strength, Yield | 9.40 MPa @Strain 300 % |
1360 psi @Strain 300 % |
ASTM D412 |
Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 H is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium sty.. |