Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 509 Butyl Sheet Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 509 Butyl Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Style #509 is a branded, chloro-butyl sheet rubber product.Information provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Oil Absorption 10 %

@Temperature 150 °C,
Time 252000 sec
10 %

@Temperature 302 °F,
Time 70.0 hour
Oil Immersion Test No. 3; ASTM D471
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
70 - 80

@Treatment Temp. 125 °C,
Time 252000 sec
70 - 80

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength >= 10.3 MPa
>= 1500 psi
12.4 MPa
1800 psi
Typical
Elongation at Break >= 350 %
>= 350 %
>= 300 %

@Treatment Temp. 125 °C,
Time 252000 sec
>= 300 %

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set 60 %

@Temperature 100 °C,
Time 79200 sec
60 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -34.4 °C
-30.0 °F