Garlock GYLON® 3522 PTFE Diaphragm

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Garlock Rubber Technologies
Trade Name GYLON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock GYLON® 3522 PTFE Diaphragm.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GYLON PTFE diaphragmWithstands aggressive chemicals and temperatures up to +500°F (+260°C).Up to four times the flex life of conventional PTFEReduced void content - less permeation, increased lifeImproved equipment efficiencyMedia: Strong caustics, strong acids, hydrocarbons, chlorine and cryogenics.Conforms to FDA regulations.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Tensile Strength 34.5 MPa
5000 psi
ASTM D1708
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C

@Pressure 5.52 MPa
500 °F

@Pressure 800 psi
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Compressibility, % 20-25
ASTM F36
Creep Relaxation, % 35
ASTM F38