Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D638 |
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet) |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D638 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D412 |
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of C.. |
|||
Tensile Strength | 34.5 - 41.4 MPa | 5000 - 6000 psi | ASTM D638 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Tensile Strength | 34.5 - 55.2 MPa | 5000 - 8000 psi | ASTM D638 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Tensile Strength | 34.5 - 41.4 MPa | 5000 - 6000 psi | ASTM D638 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Tensile Strength | 34.5 - 44.8 MPa | 5000 - 6500 psi | ASTM D638 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D1708 |
Garlock GYLON® 3522 PTFE Diaphragm GYLON PTFE diaphragmWithstands aggressive chemicals and temperatures up to +500°F (+260°C).Up to four times the flex life of conventional PTFEReduced void content - less permeation, increased .. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | across grain; ASTM F152 |
Garlock GYLON® HP3560 PTFE Gasketing, Steel Insert Gylon® with perforated 316LSS insertPerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep resistance, elim.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | across grain; ASTM F152 |
Garlock GYLON® HP3561 PTFE Gasketing, Steel Insert Gylon® with perforated 316LSS insertPerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep resistance, elim.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | across grain; ASTM F152 |
Garlock GYLON® HP3563 PTFE Gasketing, Steel Insert, Oxygen Service Gylon® with perforated 316LSS insert - Oxygen servicePerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep.. |
|||
Tensile Strength | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Michelman® Hydrosize® U2-01 Nonionic polyurethane emulsion Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2-01 is a high strength sizing for glass and carbon chopped fiber with excellent adhesion.Information provided by Michelman® |
|||
Tensile Strength | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm.. |
|||
Tensile Strength | >= 34.5 MPa | >= 5000 psi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® A1536 H (SEBS) Linear Triblock Copolymer Description: Kraton A1536 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton A1536 HU - supplied to cu.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D412 |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | across grain; ASTM F152 |
Garlock GYLON® HP3562 PTFE Gasketing, Steel Insert, Oxygen Service Gylon® with perforated 316LSS insert - Oxygen servicePerforated stainless steel core increases resistance to pressure fluctuations and thermal cyclingGYLON® offers superior cold flow and creep.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form i.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D638, ASTM D1708 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Tensile Strength | 34.5 MPa @Temperature 23.9 °C |
5000 psi @Temperature 75.0 °F |
|
Master Bond MB250NT Low viscosity ethyl cyanoacrylate Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D412 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Tensile Strength | >= 34.5 MPa | >= 5000 psi | |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
Tensile Strength | >= 34.5 MPa | >= 5000 psi | |
Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System Master Bond UV15DC80 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curin.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1050ZD96 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and .. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | 2 in/min; ASTM D638 |
Braskem FF026M Homopolymer Polypropylene Description: Excellent Color and Processing Stability, Superior Optical and Mechanical Properties, Broad Processing WindowApplications: Suggested Uses Include BOPP ApplicationsThis resin meets the r.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | ASTM D412/D638 |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde.. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | |
Henkel Hysol EA 9320NA Paste Adhesive System High shear and high peel adhesive system with room temperature cure. |
|||
Tensile Strength | 34.5 MPa | 5000 psi | |
Henkel SynCore HC 9875 Syntactic Film High crush strength, low density syntactic core material, co-curable with a variety of 350°F / 177°C curing epoxy prepregs. |