Global PP-1202-J Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PP-1202-J Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-transparency, high stiffness, high heat resistantApplications-textile applications, bags, tape, sheet, toysInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Ball Indentation Hardness 88.0 MPa
12800 psi
DIN 53456
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Shear Modulus 0.680 GPa
98.6 ksi
DIN 53457
Charpy Impact, Notched 0.400 J/cm²

@Temperature -23.0 °C
1.90 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648