Goodfellow Molybdenum 80/Titanium 20 Alloy

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Molybdenum 80/Titanium 20 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 2520 °C
4570 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 80 %
80 %
Titanium, Ti 20 %
20 %