Goodfellow Titanium 65/Aluminum 35 Alloy

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Titanium 65/Aluminum 35 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1480 °C
2700 °F
Component Elements Properties Metric English Comments
Aluminum, Al 35 %
35 %
Titanium, Ti 65 %
65 %