Gouda Vuurvast AK 85 PW Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 85 PW Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.85 g/cc
0.103 lb/in³
Apparent
Porosity 16 %
16 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 100 MPa
14500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 2.10 W/m-K

@Temperature 1100 °C
14.6 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.30 W/m-K

@Temperature 650 °C
16.0 BTU-in/hr-ft²-°F

@Temperature 1200 °F
2.50 W/m-K

@Temperature 100 °C
17.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Deformation under load - t<sub>a</sub>
1350 °C
2460 °F
Component Elements Properties Metric English Comments
Al2O3 83 %
83 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 9.0 %
9.0 %
Descriptive Properties Value Comments
Segercone 37
Thermal Shock Resistance 16 cycles
DIN 51068
Users viewing this material also viewed the following: