Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.50 W/m-K @Temperature 1100 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AC 90-5 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 1100 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 100 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 650 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 85 AM Dense Refractory Brick Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 650 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 85 M Dense Refractory Brick Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs... |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 100 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 100 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Thermal Conductivity | 2.50 W/m-K @Temperature 650 °C |
17.4 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 85 KP Dense Refractory Brick Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl.. |