Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 3.10 - 3.20 g/cc
0.112 - 0.116 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
150 - 170 MPa

@Temperature 1600 °C
21800 - 24700 psi

@Temperature 2910 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.93 - 2.13 W/m-K

@Temperature 600 °C
13.4 - 14.8 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.95 - 2.15 W/m-K

@Temperature 100 °C
13.5 - 14.9 BTU-in/hr-ft²-°F

@Temperature 212 °F
2.12 - 2.32 W/m-K

@Temperature 1600 °C
14.7 - 16.1 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1870 °C
3400 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1600 °C
-0.200 - 0.200 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 98 %
98 %
Fe2O3 <= 0.20 %
<= 0.20 %
SiO2 <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 3100 kg
Mixing Water 3.5-4.5 liters
per 100 kgs dry material