Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
MarkeTech Repton 914 Magnesia MgO REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 3.10 - 3.20 g/cc | 0.112 - 0.116 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | >= 3.10 g/cc | >= 0.112 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | After drying |
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
China Tungsten YG10X Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.10 - 3.20 g/cc | 0.112 - 0.116 lb/in³ | |
Chosun Refractories CSN-322T Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories GPB-2 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories KSB-A85 Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories SAL90 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories SAL90C Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories SAL90CR Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | |
Chosun Refractories CER-90S Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 - 3.20 g/cc | 0.112 - 0.116 lb/in³ | |
Chosun Refractories CSN-601N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.10 g/cc | 0.112 lb/in³ | After drying |
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |