Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Greene Tweed
Trade Name Avalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D792
Deformation 15 %
15 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D1457
Elongation at Break 320 %
320 %
ASTM D1457
Shear Strength 11.4 MPa

@Temperature 149 °C
1650 psi

@Temperature 300 °F
ASTM D732
13.8 MPa

@Temperature 93.3 °C
2000 psi

@Temperature 200 °F
ASTM D732
14.8 MPa

@Temperature 65.6 °C
2150 psi

@Temperature 150 °F
ASTM D732
18.6 MPa

@Temperature 37.8 °C
2700 psi

@Temperature 100 °F
ASTM D732
20.7 MPa

@Temperature 26.7 °C
3000 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.070
0.070
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.040
0.040
33.3 psi
K (wear) Factor 302 x 10-8 mm³/N-M
150 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color Bluish Black