Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed CHEMRAZ® 600 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 600 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® 600, a perfluoroelastomer, works well in both high and low temperatures. It is capable of withstanding temperatures raging from -4°F to 500°F (-20°C to 260°C). Additionally, Chemraz 600 provides good performance in hit water and steam. Because of its high durometer rating (Shore A 90), components made from Chemraz 600 offer greater resistance in high pressure and aggressive environments.Chemraz 600 has an extremely broad chemical resistance range and is made from a high-density base polymer. Chemraz 600 offers a low compression set and is perfect for sealing at high pressures. Components made from Chemraz 600 are available for use as O-rings, gaskets and many other custom shapes.Applications:Mechanical sealsPump housingsReactorsMixersCompressorsValvesInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.97 g/cc
1.97 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D1414
Tensile Strength, Yield 9.72 MPa
1410 psi
@50% Elongation; ASTM D1414
20.8 MPa
3010 psi
@100% Elongation; ASTM D1414
Elongation at Break 110 %
110 %
ASTM D1414
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: