Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.4 MPa
3250 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W780L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® H5520 High Density Polyethylene
ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® M5363 High Density Polyethylene
ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® M5370 High Density Polyethylene
ApplicationsALATHON M 5370 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. Typic..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade
ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D1414
Greene Tweed CHEMRAZ® 600 Perfluoroelastomer
Chemraz® 600, a perfluoroelastomer, works well in both high and low temperatures. It is capable of withstanding temperatures raging from -4°F to 500°F (-20°C to 260°C). Additionally..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
Teknor Apex APEX® 84129 Polyvinyl Chloride, Flexible
Notes: 80°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 22.4 MPa
3250 psi
ISO 527-1/-2
DSM Arnitel® PL461 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 22.4 MPa
3250 psi
ISO 527-1/-2
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength at Break 22.4 MPa
3250 psi
ASTM D638
Entec Hypel® PEHD8/.953 HDPE
Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec
Tensile Strength at Break 22.4 MPa
3250 psi
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive
This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making ..