Material Notes:
WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and case wear rings.WR 525 allows the pump user to increase pump efficiency by running tighter wear ring clearances, while decreasing potential pump damage when pumps are cavitated or experience down-line bearing failures.Information provided by Greene Tweed.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 86.2 MPa
12500 psi
Transverse; ASTM D3039
2070 MPa
300000 psi
ASTM D3039
Tensile Modulus 10.2 GPa
1480 ksi
Transverse; ASTM D3039
138 GPa
20000 ksi
ASTM D3039
Compressive Strength 1360 MPa
197000 psi
ASTM D695
Compressive Modulus 124 GPa
18000 ksi
ASTM D695
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: