Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 86.2 - 2070 MPa | 12500 - 300000 psi | Average value: 399 MPa Grade Count:17 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000MDHL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Global GAB-130 30% Glass Reinforced, General Purpose ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Transverse; ASTM D3039 |
Greene Tweed WR™ 525 PEEK, Carbon Filled WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D-638 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6 AF Colors Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricateAppearance: Colors AvailableInformation provi.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF5 HS L 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compos.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 04003 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass/Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES Plastiblend® ABS/PBT GF15 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000MD5L Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant (5%)Features: LubricatedForm: Pellets Information provided by Ravago. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |