Material Notes:
SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blends are found in the areas of environmental improvement (they are asbestos free) and overall cost saving. Main applications in the chemical, petrochemical, pharmaceutical, food, paper industries, etc.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Creep Strength 0.0300 MPa

@Temperature 23.0 °C
4.35 psi

@Temperature 73.4 °F
DIN 28090-2
0.0400 MPa

@Temperature 150 °C,
Time 57600 sec
5.80 psi

@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
Compressive Modulus 0.00160 GPa

@Temperature 23.0 °C
0.232 ksi

@Temperature 73.4 °F
DIN 28090-2
0.00300 GPa

@Temperature 150 °C,
Time 57600 sec
0.435 ksi

@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Chemical Properties Metric English Comments
Critical Pressure 80.0 bar
60000 torr
max
Descriptive Properties Value Comments
Color Pink
Compression Creep, MPa 17
150°C, 30 N/mm³
Leakage with Nitrogen, cm³/min 0.02
DIN 3535
Leakage, mg/s*m <.01
DIN 28090-2
max P x T , bar °C 12000
Recovery, mm 0.07
DIN 28090-2