Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | ASTM D792 |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Ferro IX 2693 Dental Glass Glass Type: Fused Silica Typical Application: Low Expansion Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also m.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | estimated by MatWeb |
Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler PTFE with graphite fillerGraphite-filled PTFE offers extremely low void content for minimal emissionsBlack GYLON® delivers long service against volatile hazardous pollutants (VHAP and VOC)Withsta.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Apparent |
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Guarniflon SC 1100 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Guarniflon SC 1400 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0201 Silica Glass Spheres Appearance: Solid clear amorphous silica microspheres with white color in powder form.Typical applications of GL0201 beads include: calibration, high temperature spacer material for gauge control, c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Schott LITHOSIL-Q Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
Polyram Metal Cap PPC371B73 Heavy Density Polypropylene, 73% Mineral Filled 73% Mineral filled, heavy density polypropylene copolymer for injection molding metalized part and galvanized covers.Information provided by Polyram. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN 53479 |
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled 73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Corning Vycor® 7907 UV-Blocking Glass Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%) Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro.. |
|||
Density | 2.20 - 2.40 g/cc | 0.0795 - 0.0867 lb/in³ | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |