Material Notes:
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Bulk Density 0.215 g/cc
0.00777 lb/in³
EN ISO 60
Density 2.20 g/cc
0.0795 lb/in³
theoretical
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Thickness 0.0500 microns
0.00197 mil
SEM/TEM
Component Elements Properties Metric English Comments
Carbon, C 96.28 %
96.28 %
XPS
Nitrogen, N 0.57 %
0.57 %
XPS
Oxygen, O 2.85 %
2.85 %
XPS
Silicon, Si <= 0.010 %
<= 0.010 %
XPS
Descriptive Properties Value Comments
Zeta Potential, mV -45.2
LD