Material Notes:
Physical Properties Metric English Comments
Density 3.80 - 4.60 g/cc
0.137 - 0.166 lb/in³
ASTM B212
Particle Size 17 - 21 µm
17 - 21 µm
10%
31 - 39 µm
31 - 39 µm
50%
53 - 63 µm
53 - 63 µm
90%
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 5.0 - 6.0 %
5.0 - 6.0 %
Chromium, Cr 2.0 - 3.5 %
2.0 - 3.5 %
Cobalt, Co 0.30 - 0.60 %
0.30 - 0.60 %
Iron, Fe 0.80 - 1.5 %
0.80 - 1.5 %
Molybdenum, Mo 2.0 - 3.5 %
2.0 - 3.5 %
Nickel, Ni 8.0 - 12 %
8.0 - 12 %
Oxygen, O <= 0.20 %
<= 0.20 %