Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 110.2 Agglomerated Sintered (Mo-Mo2C)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 516.074 Tungsten Carbide - Cobalt (WC-Co) 88-12
HS Number: 28499030 |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 527.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
|
Particle Size |
88 µm |
88 µm |
100% less than (WC-Co 83-17) |
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 584.072 Chromium Carbide-Nickel-Chromium 75-25 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than, Cr3C2 |
H.C. Starck Amperit® 585.3 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
Composition is of Cr3C2 only |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 703.1 Chromium Oxide (Cr2O3) 99.5%
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 744.3 Aluminum Oxide-Titanium Oxide 87-13 (Al2O3 - TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 745.3 Aluminum Oxide-Titanium Oxide 60-40 (Al2O3-TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 782.3 Titanium Oxide (TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 825.1 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 109.066 Agglomerated Sintered Molybdenum (Mo)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 552.074 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 558.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 742.1 Aluminum Oxide-Titanium Oxide 97-3 (Al2O3-TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 744.1 Aluminum Oxide-Titanium Oxide 87-13 (Al2O3 - TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 745.1 Aluminum Oxide-Titanium Oxide 60-40 (Al2O3-TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 782.1 Titanium Oxide (TiO2)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 516.1 Tungsten Carbide - Cobalt (WC-Co) 88-12
HS Number: 28499030 |
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 518.054 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 552.072 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni)
|
Particle Size |
88 µm |
88 µm |
100% less than |
H.C. Starck Amperit® 584.054 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
|