Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Amperit® 560.077 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 560.077 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composition is of NiSF RC 60 only
Physical Properties Metric English Comments
Density 3.80 - 4.40 g/cc
0.137 - 0.159 lb/in³
ASTM B212
Particle Size 38 µm
38 µm
Maximum 20% less than, for WC-Co 83-17
53 µm
53 µm
Maximum 10% greater than, for Ni-SF RC 60
63 µm
63 µm
Maximum 5% greater than, for WC-Co 83-17
Component Elements Properties Metric English Comments
Boron, B 3.0 - 3.9 %
3.0 - 3.9 %
Carbon, C 0.60 - 1.0 %
0.60 - 1.0 %
Chromium, Cr 14.2 - 16.5 %
14.2 - 16.5 %
Iron, Fe 3.5 - 4.5 %
3.5 - 4.5 %
Nickel, Ni 69.3 - 74.7 %
69.3 - 74.7 %
Silicon, Si 4.0 - 4.8 %
4.0 - 4.8 %
Users viewing this material also viewed the following: