Material Notes:
High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersComponents in wafer processing (susceptors, chucks, carriers)
Physical Properties Metric English Comments
Particle Size 2.0 - 4.5 µm
2.0 - 4.5 µm
Average Particle Size/Laser Diffraction D50
Specific Surface Area 2.0 - 4.0 m²/g
2.0 - 4.0 m²/g
BET
Component Elements Properties Metric English Comments
Iron, Fe <= 0.0050 %
<= 0.0050 %
Oxygen, O <= 1.5 %
<= 1.5 %