Material Notes:
FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, name plates.
Physical Properties Metric English Comments
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Yield Strength 59.0 MPa
8560 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 2.70 J/cm

@Thickness 3.17 mm
5.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 88.0 °C
190 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Flammability, UL94 HB
HB