Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO D 5302 E BLK Data provided by Multibase. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO D 6006 Grey Data provided by Multibase. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 601 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Toys; shrink films for pallets; general purpose; pipes and hoses; serum flasks. Information provided by Braskem |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
LyondellBasell Alathon® M4612 High Density Polyethylene ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Flint Hills P4G2Z-026 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Low water carryover.Applications: Extrusion: tape and strapping.Former Huntsman polypropylene products are now produced by Flint Hills Resource.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LC180 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear application.Application: Polymer modification, Shoe sole, Film coe.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Astryn CA743GA Polypropylene Copolymer Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact re.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ISO 1133 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FG5190 Linear Low Density Polyethylene FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
Melt Flow | 1.2 g/10 min @Temperature 230 °C |
1.2 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 1.2 g/10 min @Load 8.70 kg, Temperature 224 °C |
1.2 g/10 min @Load 19.2 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ExxonMobil Method |
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
after drying; ISO 1133 |
Arkema Group Orgalloy® LE 60 LM Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® LE 60LM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer Key Features: good impact and stiffness balance, good cold impact resistance, excellent dimensional stability, FDA acceptableApplications: corrugated board extrusion, appliancesMeets FDA requirement.. |