Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 44500 series sheet molding compound offers high strength and excellent resistance to corrosive agents. This compression molding grade is formulated with a vinyl ester resin system.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D572
Water Absorption 0.27 %
0.27 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
14900 psi
Flexural Strength 310 MPa
45000 psi
Compressive Strength 124 MPa
18000 psi
Izod Impact, Notched 10.7 J/cm
20.0 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 185 sec
185 sec
ASTM D495
Users viewing this material also viewed the following: