Material Notes:
A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and stainless steel alloys. Scale becomes solublized for easy removal in dilute acid.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 271 °C
520 °F
Maximum Service Temperature, Air 510 °C
950 °F
Upper limit of working range
Minimum Service Temperature, Air 371 °C
700 °F
Lower limit of working range