Polymer Property : Maximum Service Temperature, Air = 950 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 510 °C
950 °F
Pyrotek Hirolex HG Electrical Insulating Material
Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek.
Maximum Service Temperature, Air 510 °C
950 °F
Continuous
Pyrotek MCX-40 Insulating Board
MCX-40 is a bonded-mica composite for use in glass contact applications. Its high operating temperature, low porosity, and low thermal conductivity make it ideal for all areas of hot glass transfer..
Maximum Service Temperature, Air 510 °C
950 °F
Upper limit of working range
Heatbath/Park Scale Kleen 12 Descaling Salt
A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and stainless steel alloys. Scale becomes solublized for easy removal in dilute acid.Inf..
Maximum Service Temperature, Air 510 °C
950 °F
In oxygen
SGL Carbon Group EK 305 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Maximum Service Temperature, Air 510 °C
950 °F
In oxygen
SGL Carbon Group EK 40 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Maximum Service Temperature, Air 510 °C
950 °F
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled
Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material.