Material Notes:
Expanding modified epoxy film, cures at 300°F / 149°C, used for jet engine abradable fan seals.
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Modulus 0.134 GPa
19.4 ksi
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 121 °C
2.00 hour

@Temperature 250 °F
120 min

@Temperature 177 °C
2.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Out-Time (days) 10
at 32°C
15
at 25°C