Material Notes:
Turco 5948-R is an alkaline, water-based, blue, concentrated compound formulated to effectively clean painted and unpainted aircraft exterior and interior surfaces when diluted with water. Ideally suited for use on all aircraft large or small, and for cleaning engine parts during engine overhaul. It is also designed to be used in immersion tanks, for dip applications.Applications:Metal Processing LinesJet Engine CleaningAircraft Parts CleaningAircraft Depaint & RepaintAircraft Appearance
Processing Properties Metric English Comments
Processing Temperature 65.0 - 80.0 °C

@Time 900 sec
149 - 176 °F

@Time 0.250 hour
Descriptive Properties Value Comments
Chemistry Alkaline, Water-Based
Consistency Liquid
Form Concentrated
Substrate Aluminum
Ferrous
Magnesium
Non-Ferrous
Stainless Steel
Titanium