Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 25.0 - 80.0 °C | 77.0 - 176 °F | Hardening Temperature |
Möller Medical PolySkin 78 M NanoCoating Decorative coating in "metallic look," hardening at room temperature up to 80°C.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706D2 Polymer Dielectric This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706P3 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials G2020520D1 Gold Metallo-Organic Ink This is a screen printing ink designed to act as a working electrode when fired onto alumina substrates. This unique MO formulation gives a fired thickness in the order of 0.2 to 0.3 microns. This.. |
|||
Processing Temperature | 65.0 - 80.0 °C @Time 900 sec |
149 - 176 °F @Time 0.250 hour |
|
Henkel Turco 5948-R Deoxidizer Turco 5948-R is an alkaline, water-based, blue, concentrated compound formulated to effectively clean painted and unpainted aircraft exterior and interior surfaces when diluted with water. Ideally s.. |
|||
Processing Temperature | 20.0 - 80.0 °C | 68.0 - 176 °F | Chill Roll |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Hopper |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Hopper |
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar. |
|||
Processing Temperature | 70.0 - 80.0 °C | 158 - 176 °F | activation temperature used to laminate with a press or vacuum tube |
Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support.. |
|||
Processing Temperature | 70.0 - 80.0 °C @Time 3600 sec |
158 - 176 °F @Time 1.00 hour |
|
Henkel Turco 5668 Deoxidizer Turco 5668 is a diphase, liquid paint remover developed to remove resistant coatings, such as aluminized silicones, polyurethanes, acrylics, epoxies and chromated primers without using phenols, chro.. |