Hexcel® HexPly® 954-2A Curing Cyanate Resin, K1100 Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-2A Curing Cyanate Resin, K1100 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1213 MPa

@Temperature 23.0 °C
175900 psi

@Temperature 73.4 °F
Tensile Modulus 558 GPa

@Temperature 23.0 °C
80900 ksi

@Temperature 73.4 °F
Flexural Yield Strength 476 MPa

@Temperature 23.0 °C
69000 psi

@Temperature 73.4 °F
Flexural Modulus 427 GPa

@Temperature 23.0 °C
61900 ksi

@Temperature 73.4 °F
Compressive Yield Strength 262 MPa

@Temperature 23.0 °C
38000 psi

@Temperature 73.4 °F
Compressive Modulus 558 GPa

@Temperature 23.0 °C
80900 ksi

@Temperature 73.4 °F
Shear Strength 24.0 MPa

@Temperature 22.0 °C
3480 psi

@Temperature 71.6 °F