Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trade Name : HexPly® Product List

Category Epoxy Cure Resin , Carbon Fiber/Thermoset Composite , Epoxy/Carbon Fiber Composite , Epoxy/Glass SMC
Manufacturer Hexcel
Tips: Up to 50 items displayed.
PRODUCT NO. Category
Hexcel® HexPly® 8552 Epoxy Matrix, Carbon Fabric Form Carbon Fiber/Thermoset Composite
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Epoxy Cure Resin
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber Epoxy
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Epoxy
Hexcel® HexPly® 954-3 Curing Cyanate Resin Epoxy
Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber Epoxy
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M55J Fiber Epoxy
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber Epoxy
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle Epoxy Cure Resin
Hexcel® HexPly® EF01 Epoxy Structural Formulation Quick Curing System Epoxy Cure Resin
Hexcel® HexPly® EF02 Epoxy Curing System after THR 120 EF01 S50 37% Curing Cycle Epoxy Cure Resin
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2 Carbon Fiber/Thermoset Composite
Hexcel® HexPly® EH04 Epoxy Resin System, T600 Fiber Epoxy Cure Resin
Hexcel® HexPly® ES15 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2 Carbon Fiber/Thermoset Composite
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric Epoxy/Glass SMC
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Epoxy/Glass SMC
Hexcel® HexPly® F155 Epoxy Resin, T2C190 Carbon Tape Carbon Fiber/Thermoset Composite
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric Epoxy/Glass SMC
Hexcel® HexPly® F263 Epoxy Resin Epoxy Cure Resin
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Carbon Fiber/Thermoset Composite
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Epoxy/Glass SMC
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Carbon Fiber/Thermoset Composite
Hexcel® HexPly® F593 Epoxy Resin, T2G095 Carbon Tape Carbon Fiber/Thermoset Composite
Hexcel® HexPly® M20 266°F (130°C) Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 300 g/m2 Epoxy/Glass SMC
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Epoxy Cure Resin
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Carbon Fiber/Thermoset Composite
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Polyimide, TS
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber Epoxy Cure Resin
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® F263 Epoxy Resin, T3T190 Carbon Tape Carbon Fiber/Thermoset Composite
Hexcel® HexPly® F522 Epoxy Resin Epoxy Cure Resin
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Carbon Fiber/Thermoset Composite
Hexcel® HexPly® F650 Bismaleimide Resin Polyimide, TS
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Polyimide, TS
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Polyimide, TS
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Epoxy Cure Resin
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® M32 Epoxy Matrix Epoxy Cure Resin
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, High Strength 12k Carbon Balanced Fabric 600 g/m2 Carbon Fiber/Thermoset Composite
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Carbon Fiber/Thermoset Composite
Hexcel® HexPly® M65 Bismaleimide Resin Polyimide, TS
Copyright © lookpolymers.com All Rights Reserved