Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2048 MPa

@Temperature 23.0 °C
297000 psi

@Temperature 73.4 °F
Tensile Modulus 324 GPa

@Temperature 23.0 °C
47000 ksi

@Temperature 73.4 °F
Flexural Yield Strength 1034 MPa

@Temperature 23.0 °C
150000 psi

@Temperature 73.4 °F
Flexural Modulus 255 GPa

@Temperature 23.0 °C
37000 ksi

@Temperature 73.4 °F
Compressive Yield Strength 896 MPa

@Temperature 23.0 °C
130000 psi

@Temperature 73.4 °F
Compressive Modulus 290 GPa

@Temperature 23.0 °C
42100 ksi

@Temperature 73.4 °F
Shear Strength 76.0 MPa

@Temperature 22.0 °C
11000 psi

@Temperature 71.6 °F
Users viewing this material also viewed the following: