F510 150 24" EH04 38%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2080 MPa
301000 psi
Tensile Modulus 130 GPa
18900 ksi
Flexural Yield Strength 1450 MPa
210000 psi
Flexural Modulus 128 GPa
18600 ksi
Compressive Yield Strength 1510 MPa
219000 psi
Compressive Modulus 121 GPa
17500 ksi
Shear Strength 86.9 MPa
12600 psi
Short Beam