Hexcel® HexTow™ AS2C Carbon Fiber

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexTow™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexTow™ AS2C Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. Suggested for use in weaving, prepregging, filament winding, pultrusion, and molding compounds.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Filament Diameter 6.9 µm
6.9 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2140 MPa
310000 psi
Typical epoxy composite property
4470 MPa
648000 psi
Typical fiber property
Elongation at Break 1.9 %
1.9 %
Calculated from tow test data
Tensile Modulus 136 GPa
19700 ksi
Typical epoxy composite property
221 GPa
32100 ksi
Typical fiber property; Chord 6000-1000
Flexural Strength 1725 MPa
250200 psi
Typical epoxy composite property
Flexural Modulus 128 GPa
18600 ksi
Typical epoxy composite property
Shear Strength 124 MPa
18000 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 1.25
12K
2.5
6K
5
3K
Fiber Volume (%) 62
Filament Shape Round
Tow Cross-Sectional Area (mm2) 0.11
3K
0.22
6K
0.44
12K
Twist None
Weight/Length (g/m) 0.2
3K
0.4
6K
0.8
12K