Hexcel® Redux® 206-NA Foaming adhesive film

Category Polymer , Adhesive , Film
Manufacturer Hexcel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® Redux® 206-NA Foaming adhesive film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Redux 200 series is a range fo foaming adhesive films presented in sheet form. They expand during the cure cycle to fill gaps and adhere strongly to all parts of the structure with which they come into contact. Redux foaming adhesive films are compative with Redux film adhesives.Features: High strength at temperatures from -67°F to 428°F; Less than 1% volatiles emitted during cure; Suitable for aluminum and fiber-reinforced composite sandwich constructions; Expansion ratios from 1:1.9 to 1:4.0.Application: High foaming ratioAssociated Film Adhesives: Redux 312, 335, 382H, 609, 610
Mechanical Properties Metric English Comments
Shear Strength 2.00 MPa

@Temperature 80.0 °C
290 psi

@Temperature 176 °F
Aluminum Double Lap Shear (0.06 inch gap)
3.70 MPa

@Temperature 22.2 °C
536 psi

@Temperature 72.0 °F
Aluminum Double Lap Shear (0.06 inch gap)
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
Heat up rate 10°F/min
Shelf Life 18.0 Month

@Temperature -17.8 °C
18.0 Month

@Temperature 0.000 °F