Huntsman Araldite GY 508 Bisphenol A Epoxy Liquid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GY 508 Bisphenol A Epoxy Liquid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 390 to 425. Max color is 5.Comments/Applications: BPA epoxy blended with a polyglycol di-epoxide. The higher EEW allows much lower hardener levels. Flexible resin for use as modifier with other epoxy resins. Provides increased flex, elongation and impact resistance.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 2000 - 5000 cP
2000 - 5000 cP