Huntsman Araldite LZ 8001 A-80 Brominated Resin

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite LZ 8001 A-80 Brominated Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 410 to 460. Max color is 2.Comments/Applications: Bis A epoxy 80% solids in acetone (18-21% bromine). For use in manufacture of thin laminates, prepregs and rigid laminates for printed wiring boards requiring flame retardance.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1200 - 2500 cP
1200 - 2500 cP